Symbol: s
Unit: Newton per square metre (N m-2)
Stress is defined as the applied force per unit area of cross-section of a body.
![]()
This diagram shows tensile (or pulling) stress, where:
Stress can also be compressive (pushing) or shear, as shown below.
![]() Compressive stress |
![]() Shear stress |